263,344 ready Fireworks

READY Fireworks
ID Name Created On Updated On
1726713
LiBi3(P3O10)2-elastic structure optimization 2018-04-07T14:20:24.795682 2018-04-07T14:20:31.194679
1726687
Na2Ti2O5-elastic structure optimization 2018-04-07T14:20:24.767928 2018-04-07T14:20:31.194487
1726661
LiFeSiO4-elastic structure optimization 2018-04-07T14:20:18.179306 2018-04-07T14:20:31.194305
1726635
Li17(WO3)19-elastic structure optimization 2018-04-07T14:20:17.573426 2018-04-07T14:20:31.194137
1726583
P(W3O10)2-elastic structure optimization 2018-04-07T14:20:16.393584 2018-04-07T14:20:31.193785
1726557
Li32Mn13Cr3O48-elastic structure optimization 2018-04-07T14:20:16.779270 2018-04-07T14:20:31.193603
1726531
Sr9NdFe5(MoO6)5-elastic structure optimization 2018-04-07T14:20:17.813369 2018-04-07T14:20:31.193402
1726505
Na2SrV3O9-elastic structure optimization 2018-04-07T14:20:17.119342 2018-04-07T14:20:31.193232
1726479
Li2CoH12(SO7)2-elastic structure optimization 2018-04-07T14:20:15.745892 2018-04-07T14:20:31.193060
1726453
Mn(InTe2)2-elastic structure optimization 2018-04-07T14:20:16.065737 2018-04-07T14:20:31.192867
1726427
Li10Mn3V5O16-elastic structure optimization 2018-04-07T14:20:15.509176 2018-04-07T14:20:31.192701
1726401
NaCr2P2O9-elastic structure optimization 2018-04-07T14:20:14.337727 2018-04-07T14:20:31.192492
1726375
Nb3SiO10-elastic structure optimization 2018-04-07T14:20:15.059685 2018-04-07T14:20:31.192266
1726349
NaFe3P3O13-elastic structure optimization 2018-04-07T14:20:13.983594 2018-04-07T14:20:31.192100
1726297
Li20Si3P3S23Cl-elastic structure optimization 2018-04-07T14:20:13.268996 2018-04-07T14:20:31.191710
1726271
Li6MnV3(PO4)6-elastic structure optimization 2018-04-07T14:20:11.891227 2018-04-07T14:20:31.191510
1726243
Li5P(S2Cl)2-elastic deformation 23 2018-04-07T14:20:13.163849 2018-10-21T11:46:47.131501
1726241
Li5P(S2Cl)2-elastic deformation 21 2018-04-07T14:20:13.155485 2018-10-21T11:46:47.131560
1726240
Li5P(S2Cl)2-elastic deformation 20 2018-04-07T14:20:13.151374 2018-10-21T11:46:47.131589
1726239
Li5P(S2Cl)2-elastic deformation 19 2018-04-07T14:20:13.131202 2018-10-21T11:46:47.131618